Print failed because the layer adhesion is shit on my printer.

  • @rambos@lemm.ee
    link
    fedilink
    English
    111 months ago

    Sad storry dude. Do I see a skirt of that model and some brim leftovers on the build plate? Is that PLA? Are you using glue?

    • GregorTacTacOP
      link
      fedilink
      English
      111 months ago

      No, I didn’t use a skirt or brim. Good idea, I’ll use it next time. I’m using PETG as my filament and no, I’m not using glue.

  • @Starb3an@sh.itjust.works
    link
    fedilink
    English
    511 months ago

    Completely off topic: I now dry all of my filament for about 10 hours in a cheap food dehydrator before I print. Print quality is 1000x better.

  • atocci
    link
    fedilink
    English
    211 months ago

    Yeah I think you need a new build surface, friend.

      • @EmilieEvans@lemmy.ml
        link
        fedilink
        English
        311 months ago

        As cheap as $2 from Ikea for a mirror or roughly $15 for a PEI sheet. Print surfaces are consumables like nozzles or filament.

        This print bed has seen better days but doesn’t need to be replaced right now.

        Btw. Using PETG on glass or Creality glass surfaces is a great way to destroy them in a timely manner.

        • @beastlykings@sh.itjust.works
          link
          fedilink
          English
          111 months ago

          This is very informative thanks. I’ve printed a lot of PLA on my Creality glass plate with no issues, but I recently started with PETG and it’s insane how much harder it sticks.

          I learned through trial and error to only remove it while the bed is still hot, but even then it really sticks too well.

  • @rugburn@lemmynsfw.com
    link
    fedilink
    English
    511 months ago

    I don’t know what it is with ender build plates but they only seem to last about 30-ish prints on the PEI side for me, switched to the glass side and glue stick with moderately better results

    • GregorTacTacOP
      link
      fedilink
      English
      211 months ago

      A lot of printing. It’s basically impossible to clean it well.

      • AmbiguousProps
        link
        fedilink
        English
        211 months ago

        Are you removing your prints when the build plate is still hot? If so, and your plate is PEI, it’ll get destroyed

          • GregorTacTacOP
            link
            fedilink
            English
            311 months ago

            I second that. Mine worked for quite a bit of time until it stopped working properly.

            • @wjrii@lemmy.world
              link
              fedilink
              English
              111 months ago

              Glue stick helps, as does cleaning with ISO between every. single. print. Also praying.

              I got an old school build-tak style sticker for one of my glass beds once I finally got sick of it. Ender 3 style glass beds are just bizarre, ornery little things.

              • @morbidcactus@lemmy.ca
                link
                fedilink
                English
                211 months ago

                Buildtak is fantastic, I’ve swapped over to all buildtak on my voron and for abs on my prusa, A little bit of 99ipa between prints and you’re good, never had to worry about adhesion. I had a glass bed on a Mendel Max 2 literally a decade ago that I ended up selling about a year later when I moved cross country, ignoring bed leveeling and z axis issues I had, adhesion was always a mess, ended up doing the coat in polyimide tape and gluestick thing with success but it was always a bit how you doing. It’s great how far things have come.

      • @AnarchoSnowPlow@midwest.social
        link
        fedilink
        English
        111 months ago

        With that one (creality textured glass carborundum something or other) I kept hitting it with 95%+ IPA, it just gives out eventually. I switched to a textured spring steel plate recently, world of difference for petg, PLA, and tpu. It’s just another consumable :/

        If you’re not ready to switch yet a layer of masking tape can get you by for awhile, it’s just a pain because the masking tape will need to be replaced about every other print depending on your settings.

  • @EmilieEvans@lemmy.ml
    link
    fedilink
    English
    411 months ago

    Scraped a 600g print for the second time (today):

    first failure: bed adhesion/warping

    second failure: Prusaslicer overlapped support and the part. At least my hotend survived that failure.

    Called it a day and moved on to a different printer for this print. Also, did I mention that I managed to kill another z-endstop on that printer today? Forgot to remove a finished print before running G28.

      • @EmilieEvans@lemmy.ml
        link
        fedilink
        English
        311 months ago

        The end stop is located on the carriage (toolmount/receiver). Moved sideways into the print and the bed adhesion was stronger than the pin of the switch.

  • @Dumnorix@lemmy.world
    link
    fedilink
    English
    411 months ago

    If printing PLA, put a brine (salt solution) on your bed. PLA bonds with salt when warmed up (heated bed) and loses its bond when cooled off.

  • Carighan Maconar
    link
    fedilink
    English
    711 months ago

    Thanks, I was considering what to make for dinner, and spaghetti it shall be!